Welding in 6061 T6 aluminium alloy

45 views
Skip to first unread message

Bhima Kanjariya

unread,
Oct 25, 2019, 1:35:05 AM10/25/19
to Materials & Welding
hello friends

We have one aluminium alloy Bucket used in Urea Prilling tower (pics attached for reference)

We found a through crack in T-joint fillet welding of two plate

please advise how to weld and also suggest party who expert in welding aluminium


Thanks in Advance

Bhima Kanjariya
IMG_20191022_180928.jpg

Karthik

unread,
Oct 25, 2019, 3:18:10 AM10/25/19
to Materials & Welding
Hi,
The attached file might be useful to you.

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

E-mail : karthi...@yahoo.com



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f5e16324-906c-42b0-a626-6b321bb17fbc%40googlegroups.com.
Aluminium alloy welding and fabrication.pdf

Bhima Kanjariya

unread,
Oct 28, 2019, 5:32:40 AM10/28/19
to Materials & Welding
Thank you

if possible please provide party contact who expert in doing Al welding
Reply all
Reply to author
Forward
0 new messages