Regarding Post Heating or Post Baking

33 views
Skip to first unread message

Mohit Aggarwal

unread,
Apr 11, 2017, 12:38:55 AM4/11/17
to materials-welding
Dear Experts,

Kindly share the standard or code in which there is mention about post Heating of Alloy Steep materials like 
SA 335 P5 and SA 335 P9 etc.

Regards,
Mohit Aggarwal
9821958461

Prasad Rode

unread,
Apr 16, 2017, 2:28:26 AM4/16/17
to Materials & Welding
Dear Sir,
post heating, it may or may not be mentioned in code, but it is good engineering practice to performed the post for 1 hr.

It prevents the joints from cold cracking.

Kannayeram Gnanapandithan

unread,
Apr 16, 2017, 6:24:57 AM4/16/17
to materials-welding
Check in ISO 1011-2

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPNOQS0jNPgxPwQgmMY1bn4WLnG2x00WsFVN%3DPuFC9U37Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

C.Muni

unread,
Apr 16, 2017, 11:41:16 AM4/16/17
to material...@googlegroups.com
Post heating is  required for P91 material to avoid cracks.Other materials not required


--

Kannayeram Gnanapandithan

unread,
Apr 16, 2017, 9:36:41 PM4/16/17
to materials-welding
Muni, it is not like that only p91 required. Other Steel materials also required Based on CE, Hardness, thickness etc. Pl ref ISO1011-2 for further details information