Impact Test requirement for multi process PQR as per ASME SEC IX / B31.3

143 views
Skip to first unread message

Prakash Pugazhenthi

unread,
Mar 2, 2024, 2:45:43 AM3/2/24
to Materials & Welding
Hi all i have an query for Impact Test requirement for Multi Process PQR.

We have an requirement of Impact Test for LTCS PQR. How to select Impact specimen location. Whether we have select for process wise or both process combined in single specimen or for GTAW is enough.

The below are the details.

Coupon Size: 10" x 9.27mm thickness
Material: A333 Gr.6 to A350 Gr.LF2
Process: GTAW + SMAW
Filler metal: ER80SNi1 + E7018-1
Deposited Weld Metal: GTAW - 3.5mm and SMAW-5.77mm

Client specification refers B31.3. 

DEEPAK KASHYAP

unread,
Mar 2, 2024, 3:46:31 AM3/2/24
to material...@googlegroups.com

Dear Mr. Prakash,

 

As per your query, please find the reference snap of B31.3, however as per my understanding both Processes Weld and HAZ subsize samples shall be taken individually.

 

 

 

Thanks & Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eac62c50-8e7d-4448-911f-4313c2826f25n%40googlegroups.com.

image001.png
Reply all
Reply to author
Forward
0 new messages