Right consumable for S 31254 to SA 516 Gr 70 mtrl.

21 views
Skip to first unread message

clvaid...@gmail.com

unread,
Jun 30, 2020, 5:09:57 AM6/30/20
to Materials & Welding
Right consumable for S 31254 to SA 516 Gr 70 mtrl.

Karthik

unread,
Jun 30, 2020, 6:47:47 AM6/30/20
to Materials & Welding
Hi,
S31254 is under ASME P.No.8. SA516 Gr.70 is P.No.1.

For P.No.8 to P.No.1 use E/ER309 or ER309L

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

E-mail : karthi...@yahoo.com



On Tuesday, June 30, 2020, 04:39:00 PM GMT+7, clvaid...@gmail.com <clvaid...@gmail.com> wrote:


Right consumable for S 31254 to SA 516 Gr 70 mtrl.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e7b82fda-3f60-437d-863d-acb7a18349fco%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages