Dear all,

What Test is required for filler wire as per ASME section II part C and what dimensions we have use for testing plate for filler.



Best regards.
SUJIT

Vishwas Keskar Welding Manager WELDING

unread,
May 17, 2023, 3:34:28 AM5/17/23
to Materials & Welding
Which specification and AWS  wire ?

Pl refer respective specification/AWS name for required tests  in ASME SEC II C 

The consumable mfg er  will issue certificate as per that specification .

If you need particular batch to be tested  and need results which was shipped to you , this requirement  shall be addressed in Consumable PO thr TDC

Thanks
Vishwas -IWE 

sujit kumar

unread,
May 17, 2023, 4:15:03 AM5/17/23
to vvkes...@gmail.com, material...@googlegroups.com
Dear 

Vishwas Keska


SFA NO-5.9
AWS NO-ER316L, ER347,ER308L,

SFA NO-5.14
AWS NO-ERNICr-3

Please find the above sfa no and aws no for your reference.please explain what test require as per asme section II part C.


Thanks & Regards
Sujit

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b1d21064-2722-4a64-a3c9-9793bbcfa3b7n%40googlegroups.com.

Srinivas Rao

unread,
May 17, 2023, 4:20:46 AM5/17/23
to Materials & Welding
pls refer ASME Sec IIC , with  referance to AWS classification of each filler wire /Electode  and  refer SFA 5.01 for testing requiremnts and refer respective SFA for test coupons prepation based on different testing requiremnts .

regards 
Srinivas Rao
Welding Engineer 

james gerald

unread,
May 17, 2023, 6:14:04 AM5/17/23
to material...@googlegroups.com
Only Chemical Analysis

Thanks & Regards

J.Gerald Jayakumar