dissimilar material contact with each other like- stainless steel contact with carbon steel

64 views
Skip to first unread message

Rameez khan RK

unread,
Jun 29, 2020, 4:07:15 AM6/29/20
to Materials & Welding
Dear Experts,
            can any one tell me what is the cause if ss (stainless steel) in direct contact with cs (carbon steel). could anyone please define me as per standards and code.

Thank you 
RK  

George Dilintas

unread,
Jul 2, 2020, 12:05:41 AM7/2/20
to material...@googlegroups.com
One tadvise : never write "ss". This is reminding Hitlers murderers . When CS comes in contact with Stainless Steel the protective layer of stable Cr Oxide is destroyed,  On the top of that the traces of CS do not allow the Cr to come into contact with O2 to create again the protective Cr Oxid layer and thus corrosion is initiated. This phenomenon is called "iron contamination".
I don't know if there is any Code or standard. However, this is basic metallurgy and corrosion knowledge.
Don't forget that there is no substitute to engineer's judgement.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e2f17873-860c-43a3-a252-a4f9cfd6ee4fo%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

atul khatri

unread,
Jul 2, 2020, 12:46:57 AM7/2/20
to material...@googlegroups.com
In addition to George's response , please don't overlook the " Galvanic Corrosion" if the below mentioned conditions exist in your case. 

           1. The metal joint must be wet with a conductive media (probable liquid media, or humid gas)
           2. There must be metal to metal contact
           3. Sufficient different potential between the metals in contact

All three conditions shall exist for galvanic corrosion.

 For more detail on potential differences between metal refer  "Astm G82 (Development and use of a galvanic series for predicting galvanic corrosion performance)"