GRP Information

41 views
Skip to first unread message

Ahmed Rashed

unread,
Dec 26, 2021, 11:46:57 AM12/26/21
to material...@googlegroups.com

Dear all,

Hope to be in a good health

I need to know how can i make material receiving for GRP piping and fitting 

Like which standard to check the dimension of piping and fitting ( ovality , length , thickness ..etc)

Thanks in advance

Mohd Siraj

unread,
Feb 7, 2022, 4:18:42 AM2/7/22
to Materials & Welding
for GRP, use only manufacture tolence,

who is your supplier?  CPI or else.

mfg is providing dia and thk tolenrece bassed their process to make this pipe, fitting , t connection, as you know all are made from grp filament have difference tolerance mfg to mfg.

for other qualification work also u can request their procedure or MOS.