My question is as per ASME SEX-IX,

MINIMUM WELDER QUALIFICATION THICKNESS RANGE WHERE IT IS GIVEN ?

Best Regards,

BHASKAR.

hardik desai

unread,
Feb 13, 2017, 6:14:11 AM2/13/17
to material...@googlegroups.com
QW-452.1(b)

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/df357b7b-5342-44c9-8a08-3f4ba67b9e7d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

George Dilintas

unread,
Feb 17, 2017, 9:45:26 PM2/17/17
to Meghanadh K
there is no minimum deposited metal thickness for the welder. Only maximum to be welded.
The minimum depends only on the applicable WPS


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/df357b7b-5342-44c9-8a08-3f4ba67b9e7d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Mohd Siraj

unread,
Mar 8, 2017, 5:17:19 AM3/8/17
to Materials & Welding
Min as per wps is qualifie And maximum 2t.