Corrosion Rate criteria for material UNS N06022 nickel alloy

74 views
Skip to first unread message

Vivek

unread,
Dec 2, 2024, 5:09:50 AM12/2/24
to material...@googlegroups.com
Team,
This is regarding material UNS N06022.

The corrosion Test is carried out as per ASTM G28 Method A.
The test result is 37.762 mpy (0.9592 mm/year).

May I know which standard provides acceptance criteria (range) for corrosion rate?

Regards,
Vivek

israr

unread,
Dec 27, 2024, 7:29:40 AM12/27/24
to Materials & Welding
Corrosion Rate required based on the process fluid,
Client has to provide