There is not much difference.
Both are assuring quality for the project before starting .
Different countries users use different terminology.
Can any one provide me a details explanation of difference between QAP and ITP.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d5107353-54a0-49a9-9d23-6123ee54d599%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
They are different terminology used in industry but the intent remains the same. The basic purpose is to outline all the activities of manufacturing the product.
Regards,
Vino
Can any one provide me a details explanation of difference between QAP and ITP.
From: Mohammed Ghani Sent: Σάββατο, 16 Ιανουαρίου 2016 - 17:43 Reply To: material...@googlegroups.com Subject: Re: [MW:24106] what is the difference between QAP and ITP |
Mr. George Dilintas,
The one you are specifying as QAP is called in some industry as PQP and that is the Project Quality Plan.
I don't think that such terminology are defined in any Construction Code, but possibly in ISO 9001 Standard.
Regards
Vino, Doha
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OF1707FED7.4F2CA247-ONC1257F3D.002A2E4A-1453016444003%40LocalDomain.
Can any one provide me a details explanation of difference between QAP and ITP.
Hi,
ITP – Inspection test plan includes tests, its acceptance tolerance, type of instruments used, its accuracy etc –
Ex –
Pipe thickness – ultrasonic method, XXX instrument, nominal thickness 10mm, acceptable “-0mm +1.6mm” etc, frequency each pipe measured from outside, at 6 locations, procedure for testing – as per Doc # - XXXXX
ITP is a in house document of a manufacturer. (in some complicated cases, and close tolerance requirement cases clients asks for ITP also)
In ITP manufacturing process also defines, but where as in QAP it is not required.
Whereas QAP means it’s a quality plan and broad details will be their…
Ex- Pipe,
Thickness, Dia, Length
Frequency – each pipe
Acceptance norms – Client spec / ASTM code / Project spec / approved drawing etc
Client witness / TPI witness etc
QAp is a client approval document.
Thanks & Regards,
Lakshman Kumar B,
From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Kadir godil
Sent: Tuesday, January 19, 2016 8:45 AM
To: material...@googlegroups.com
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKaLp%2BVeSfvN1fLsv_-qmu0uPZk4C_HpwW305agu3y9TgPM-YA%40mail.gmail.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM7oz7DeOS3RJQ-a0PWqtR-sHM1ZhSaZGS1GcJSk1_X2V0nibQ%40mail.gmail.com.
Dear Sirs
QAP :- Usually describes how will you manage the Quality System
Eg:
1. Project Management strategy
2. Applicable documents
3. Management system & Responsibility
4. Project execution
5. QA/QC
6. Marketing, design, Procurement ,Production, store
7. Resource management
8. Product realization
9. Measurement analysis &improvement
10. HR & logistics
11. Project Organogram
ITP:-solely related to QA/QC this will describe all the various stages of inspection and testing from start to finish requirements of a product.
Generally this will include monitoring, Review, witness and hold points listed for all relevant parties and this is approved prior to commencement
Regards
M.S Nair.G
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/002801d15279%247cc6f870%247654e950%24%40com.
Dear all,
QAP says "who will do, what will be done by whom etc" mainly designation and job responsibilities.
ITP says "how much to be done, when to be done, what record to be made etc" mainly work related activities, their controlling documents and inspection frequencies.
Regards,
Hareesh K V
+8547859202
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE12Qq7HUCj5CAASB%2B5OW_P71npZ%2B1wU%3DJk7-O1ShgLvj%3DpnNg%40mail.gmail.com.
Do not stick to definitions and abreviations.
Focus to the point...
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS HELLAS A.E - PIRAEUS GREECE
Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Kannayeram Gnanapandithan ---19/01/2016 15:27:10---go with Mr George Lintas THANKS & BEST REGARDS,
.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNf6hxueH7cK0Z4b%3DOBU%3DrnAQBct%3DAu76yQbS7dJYejBA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.