Dear Experts...Please Explain.

How to get magnetization for carbon steel material (like...A53,A106,API 5l) during fit up fabrication activity  and how to rectify to proceed welding works.

Eyup Tan

unread,
Jun 26, 2019, 5:14:20 AM6/26/19
to material...@googlegroups.com
See attachment

Best Regards,

Eyup Tan



On Tue, Jun 25, 2019 at 2:27 PM <cha...@gmail.com> wrote:
Dear Experts...Please Explain.

How to get magnetization for carbon steel material (like...A53,A106,API 5l) during fit up fabrication activity  and how to rectify to proceed welding works.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d497bb84-e84b-446e-8676-6fbd80eaca9e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
DEMAGNETIZATION OF PIPE MAGNETIZATION.pdf
Reply all
Reply to author
Forward
0 new messages