Dear All
What type of Pentameter should i use during Radiography Test of a butt weld joint of 50 mm diameter & 12 mm thickness and joint between A182 F91(WN Flange) to SB622 UNS N10276(Pipe).
Regards
Subrata Das
It should be penetrameter, and the term penetrameter no longer used in Article 2 of ASME Section V now it is being referred as image quality indicator (IQI). You can select the IQI material from the less radiation absorbing material out of this two (material group 1, CS or SS will do).
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.