how is repair calcualted in piping percantage of RT IS 5%

44 مرّة مشاهدة
التخطي إلى أول رسالة غير مقروءة

attaulla khan

غير مقروءة،
22‏/01‏/2023، 9:37:42 م22‏/1‏/2023
إلى Materials & Welding
Dear gents i have attached a excel sheet of repair  rate welder wise can any one help me in these figures my doubt is how did get this with out lenth of of repair
the percentage of RT is 5% 
P10568-RepairStatusByWelder_20-01-2023.xls

james gerald

غير مقروءة،
23‏/01‏/2023، 10:21:29 م23‏/1‏/2023
إلى material...@googlegroups.com
The acceptable Repair percentage is specified in the Client specification.

From your Excel sheet as below.

Inline image


From your attached sheet, the Repair percentage is calculated in 2 ways.

1. Joint wise (no of Joints Repair / Total no of Joints RT shoot x 100).
2. RT Film wise ( no of Films Repair / Total no of Films shoot x 100).

From the Client specification, you can understand what is the 5% limit.

Thanks & Regards

J.Gerald Jayakumar




On Monday, 23 January, 2023 at 05:37:37 am GMT+3, attaulla khan <attaul...@gmail.com> wrote:


Dear gents i have attached a excel sheet of repair  rate welder wise can any one help me in these figures my doubt is how did get this with out lenth of of repair
the percentage of RT is 5% 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cb8e9fbc-4ac3-4220-b95e-b43086acd974n%40googlegroups.com.
الرد على الكل
رد على الكاتب
إعادة توجيه
0 رسالة جديدة