Dear All,

As material test cerificate  of welding consumables does not specify validity period for welding consumable, then what is the thumb rule to consider it.

I had checked ESAB Handbook ,it states that max 3 years for electrode if stored as per their guidelines but nowhere i had found information regarding max storage time for filler wire.

Can anyone put light on this topic

Regards,
Afroz Shaikh
IOTIES

MUNHOZ Sergio TECHINT

não lida,
20 de jan. de 2016, 04:43:4820/01/2016
para material...@googlegroups.com

Welding consumables  can be recertified  by the manucturer after expiration date.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/dce3f397-66ba-4993-bd35-86c1c5507cfc%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Perumal Govindan

não lida,
21 de jan. de 2016, 07:57:5821/01/2016
para material...@googlegroups.com

Hi,
Maximum one year shall be advised / permitted to use the welding consumables from the date of manufacturing.

With kind regards
Govindan

--

Babu Kathalingam

não lida,
21 de jan. de 2016, 07:58:0021/01/2016
para material...@googlegroups.com

You can use as long as it is in good condition

--

Nachhattar Singh

não lida,
21 de jan. de 2016, 09:02:3821/01/2016
para material...@googlegroups.com

Dear Friends

 

For how many times you can bake and use the welding Electrodes?

Thanks  

 

Nachhattar Singh

 

PLEASE THINK BEFORE PRINTING

afrozsh...@gmail.com

não lida,
22 de jan. de 2016, 07:21:4422/01/2016
para Materials & Welding
max 3 times

MUNHOZ Sergio TECHINT

não lida,
22 de jan. de 2016, 07:24:0822/01/2016
para material...@googlegroups.com

It is defined according to the manufacturer instructions and consumable specification; usually no more than twice.

 

Best Regards

Kannayeram Gnanapandithan

não lida,
22 de jan. de 2016, 22:16:2022/01/2016
para materials-welding

Follow manufacturer recommendation

Maulik Thakkar

não lida,
23 de jan. de 2016, 08:47:1423/01/2016
para Materials & Welding

Dear sir,

Recommended to follow material data sheet provided by manufacturer.

Above given limit it is user's responsibility to check performance of consumable as to ensure quality.

Life of consumable is normally depends on:
1. Manufacturer.
2. Storage condition.
3. Type of consumable.

Regards,
Maulik