Piping WPS/PQR and Welder Qualification Compliance- ASME IX or ASME B31.3

1,310 views
Skip to first unread message

Anban

unread,
Sep 13, 2015, 12:24:46 AM9/13/15
to Materials & Welding
Dear Sirs
Appreciate if you could provide clear and definitive response.

In my Yard Piping WPS/PQRs and Welders Qualification comply with ASME IX only.

ASME IX specifically developed as  Qualification Standard for Welding,Brazing, and Fusing Procedures;Welders; Brazers; and Welding,Brazing, and Fusing Operators
ASME B31.3- ASME Code for Process Piping.- (Design/Construction Code)


As For Welder/Operator/Brazer Qualification& Piping WPS/PQR Qualifications- what is mandatory code- ASME IX or Design/Construction Code ASME B31.3?


For example High Pressure Piping ASME B31.3 Chapter IX shall be complied for WPS/PQRs and Welder Qualifications.
Yes, PWHT requirements one need to comply with ASME B31.3-Table 331.1.1

Does that mean ASME IX requirements superseded by ASME B31.3 Chapter IX?
Where and when one shall comply with ASME B31.3 instead of ASME IX.?


Thanks


Raghuram Bathula

unread,
Sep 13, 2015, 12:29:10 AM9/13/15
to Materials-Welding
You need to follows your code of construction (B31.3 in your case) in addition to ASME BPV IX. If piping is designed to B31.3, then you need to follow the requirements of B31.3

Kannayeram Gnanapandithan

unread,
Sep 13, 2015, 12:51:04 AM9/13/15
to materials-welding
follow construction code  in addition to sec 9

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ecf4c1ee-a46c-4bd7-aec7-2ba942eaa094%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

george....@gr.bureauveritas.com

unread,
Sep 13, 2015, 3:01:02 AM9/13/15
to Anban
Design and construction Code requirements have  prevalence

Sent from my BlackBerry 10 smartphone.
From: Anban
Sent: Κυριακή, 13 Σεπτεμβρίου 2015 - 07:24
To: Materials & Welding
Subject: [MW:23463] Piping WPS/PQR and Welder Qualification Compliance- ASME IX or ASME B31.3

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ecf4c1ee-a46c-4bd7-aec7-2ba942eaa094%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Kannayeram Gnanapandithan

unread,
Sep 13, 2015, 3:53:17 AM9/13/15
to materials-welding
as far as B31.3, it does have all variables for which it refers to Sec9

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

Sudhakar Kuppuswamy

unread,
Sep 14, 2015, 1:53:58 AM9/14/15
to google welding

Hi,

Please note, ASME section 09 is not a design code, it is just a supporting document for other ASME Design/Construction Code. Only Design/Construction codes such as ASME B31.3, ASME 31. 1, ASME Section 08 Div. 1, 2, 3 & ASME B31.4, ASME B31.8 etc. provides the rules for fabricating a component not the ASME Section 09.

The Design/Construction code requirements come on the top, in the hierarchy of fulfilling the requirements. In your case you need fulfill the requirements of ASME B31.3.


Thanks and regards,


Sudhakar.K



Kannayeram Gnanapandithan

unread,
Sep 15, 2015, 5:38:38 AM9/15/15
to materials-welding
pl ref ASME B31.3, 328.2 & 328.2.2 for welding qualification , it is clear that u have to carry out qualification as per Sec 9 plus additional requirement of B31.3

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

NARK

unread,
Feb 5, 2020, 4:14:24 AM2/5/20
to Materials & Welding
All the qualifications are conformed with ASME Section IX,But if any conflict arises with IX and B31.3,in this case B31.3 (CONSTRUCTION CODE) supersede all the requirements.

Example Qualification by others is prohibiting by section IX(INTERPRETATIONS IX-95-27 & IX-98-02)
But B31.3 accepting the qualification by others clause 328.2.2(INTERPRETATIONS 31.3-26-34)

Interpretation 26-34 
Subject: B31.3-2016, Interpretation of Para. 328.2.2 Ownership of Welding Procedures 
Date Issued: April 11, 2018 
File: 18-164 

Question 1: In accordance with ASME B31.3-2016, may a contractor follow a WPS that has been qualified by another company in accordance with the requirements of para. 328.2.2? 

Reply 1: Yes. 

Question 2: In accordance with ASME B31.3-2016, does para. 328.2.2 take precedence over the rules of ASME Section IX? 

Reply 2: Yes.  

IN CASE OF IMPACT TEST THICKNESS FOR PIPING -ASME 31.3 SUPERSEDE THE ALL REQUIREMENTS.(T/2 TO T+6 MM) CHAPTER 3