SS304 HEAT TREATMENT PROCEDURE

62 views
Skip to first unread message

Ganesh Rao

unread,
Mar 19, 2023, 10:59:22 PM3/19/23
to Materials & Welding
Dear Expert,

We looking for PWHT Procedure for material SS304.could any one can share the procedure urgently?
Pipe thickness : 10mm
Pipe OD : 1260mm
We need to do hot tapping on this pipe 


From,
Ganesh

biennd

unread,
Mar 19, 2023, 11:23:53 PM3/19/23
to Materials & Welding
Solution heat treatment follow quenching.
You also see in material spec ASTM A312 TP304.
Regarding rolling from plate with 10mm. it may not apply PWHT for this material type.

james gerald

unread,
Mar 20, 2023, 7:09:52 AM3/20/23
to material...@googlegroups.com
Are you referring to Base Metal heat Treatment or weld Heat Treatment, for the former case as per ASME IIA SA240 for SS plates and for the latter no Heat Treatment is required.

Normally you use a Split Tee for large dia Hot Tap and a Weldolet for dia upto to 2inch and the weld do not require PWHT.

Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/54d9870d-05e5-46b4-9547-5a9edf162811n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages