Thanks & Regards
J.Gerald Jayakumar
Dear Expert,we have some pipes of 316 material all pipes are off cut and heat identification is not available on these pipes. MTC type requirement is 3.2 also we have not MTC. what is the Procedure to certify the material as per the 3.2 type requirement?