Weld Copper to Stainless Steel 304

79 views
Skip to first unread message

Sohil Mehta

unread,
Jul 30, 2022, 10:00:55 AM7/30/22
to Materials & Welding
Dear Sir, 

Kindly suggest consumables for welding of Copper to Stainles Steel. 

Thank you.

Regards,
Sohil Mehta

Mohd Siraj

unread,
Aug 11, 2022, 9:31:22 PM8/11/22
to Materials & Welding
pl share exact specification of material to be weld with thickeness.

for any question to be answered quickly , you could provided suffiecent details so that other can understand your requirement like code interpretation querry.

J Prinsen

unread,
Aug 25, 2022, 8:25:54 AM8/25/22
to materials-welding
You can try with inconel 625 or Nickel 200, or buttering the stainless steel with either 625 or 200 and then weld with the same consumable  to the copper
I' ve seen welding with a copper consumable in the past, but there is a high risk of hot cracks


Regards

Jurgen Prinsen IWE

Van: "Mohd Siraj" <mohd...@gmail.com>
Aan: "materials-welding" <material...@googlegroups.com>
Verzonden: Donderdag 11 augustus 2022 17:09:48
Onderwerp: [MW:33377] Re: Weld Copper to Stainless Steel 304

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c84d8a39-6385-4d7d-9c48-df32d4658770n%40googlegroups.com.

Prakash Hegde

unread,
Aug 25, 2022, 11:45:13 PM8/25/22
to material...@googlegroups.com
My opinion with experience Copper to SS welding is not compatible
You can braze or vaccine braze with BAg8 or similar  filler

George Dilintas

unread,
Aug 25, 2022, 11:45:16 PM8/25/22
to material...@googlegroups.com
Copper and Steel never formed solid solution. Try with Nickel buttering on both parts and then join with nickel 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

pgos...@rogers.com

unread,
Aug 26, 2022, 12:05:02 AM8/26/22
to material...@googlegroups.com

Arc Welding is difficult, Brazing is possible. If fact a of copper to stainless joints are Arc Brazed with Silver Brazing filler . BAg 8 as cited by Mr Hegde  is a popular filler metal for such brazing. The most common option for joining  simpler shapes is Friction Welding , example as shown below.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Cell/Whasapp:1-905-9793232

image002.png

Kannayeram Gnanapandithan

unread,
Aug 26, 2022, 1:52:35 AM8/26/22
to materials-welding
butter copper with Monal or Cupronickel, and the weld with Stainless steel

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


Reply all
Reply to author
Forward
0 new messages