Hi Cast Irons are typically subjected to repair weld. The repair welding is normally done by Nickel based electrodes, 99% Ni or 55% Ni electrodes. This applies to any welding on new cast iron pipes also. It’s extremely difficult to meet ASME Sec-IX welding qualification criteria for Cast Iron Welding.
The links cited below would provide you good resources for Cast Iron Welding.
Thanks.
Pradip Goswami.P.Eng, IWE.
Independent & Consulting Welding & Metallurgical Engineering Specialist
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
Email:pgos...@rogers.com,pradip....@gmail.com
Cell/Whasapp:1-905-9793232
Can You Weld Cast Iron? (A Complete Guide) - TWI (twi-global.com)
From: luis carlos greggianin <luisca...@gmail.com>
Sent: March 25, 2021 5:53 PM
To: material...@googlegroups.com
Subject: Re: [MW:32090] ductile iron welding procedure
Use shot penning during the weld too
Em Qui, 25 de mar de 2021 00:13, QA/QC <adnan...@gmail.com> escreveu:
Dear master
in our project we have a leak in fire water service and I want to know the repair procedure for the pipe
ductile iron C151A21.51
electrode rod using for and procedure if possible
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bd7269bd-a954-4c54-a816-2c3c45a84f3bn%40googlegroups.com.