Pitting corrosion acceptance criteria for steel plates

162 views
Skip to first unread message

KrishnaMoorthy ChinnaSamy

unread,
Jan 31, 2022, 10:16:08 PM1/31/22
to Materials & Welding
Dear,
Is there any allowances or acceptance criteria for pitting corrosion in offshore structural plate material (S355 JR)…
And also how to measure the depth of pitting size…
Kindly advise…
Thanks & Regards 
KrishnaMoorthy

Mohd Siraj

unread,
Feb 6, 2022, 7:01:05 AM2/6/22
to Materials & Welding
1) check wirh welding guage
2) UT thickness machine
3) or if more deep, u can use piano wire technich and scale( non coventional but practicle method)