2" PIPE PQR

38 views
Skip to first unread message

mmm

unread,
Apr 5, 2017, 4:50:24 AM4/5/17
to Materials & Welding
Dear Experts

i have to prepare test specimen for 2" pipe for which i have to recommend two tensile test and 4 bend test as per secIX and B31.3

1) how many test piece required to complete these test  as circumference of 2" pipe is 190mm

2) in case of one tensile test fails and another is passed, do i need to consider the whole PQR is failed or only that test specimen is failed, please clear my doubt.


Thank you

George Dilintas

unread,
Apr 5, 2017, 8:21:29 AM4/5/17
to Meghanadh K
you don't need to make the PQR on a pipe, since diameter in ASME is not an essential varaible for rocedure qualification.
If one test fails then you repeat the PQR

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bc58b053-0342-426d-a659-12e151616837%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Perumal Govindan

unread,
Apr 6, 2017, 12:48:37 AM4/6/17
to material...@googlegroups.com

Hi

Please take three test coupons for PQT.

In case if one test specimen fails with tensile test you can go ahead for testing with additional specimen without a new PQR.

Regards
P Govindan

--