Hi Everyone,
I am new to welding engineering. I just want to know the F number, Base material and Process co-relation table. Is there ant details available in Section 9
Thanks
Asir
Karthik
unread,
Jan 17, 2023, 5:28:00 AM1/17/23
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
Hi,
F number is a filler material Number specified in ASME Sec.IX. Select correct Fillet material from consumable from manufacturer's catalogue for LTCS material, and refer Table QW 432 of ASME Section IX for F number