Golden weld requierements

85 views
Skip to first unread message

raouf salhi

unread,
Apr 26, 2017, 6:19:09 AM4/26/17
to Materials & Welding
Dear experts ;

We have a power piping project ( B31.1 ) and our subcontractor is only performing RT or UT for golden weld , I know that it should be full NDE but I can't find this requirement in the code .
Can somebody give me the exact requierements for golden weld ?

Many thanx

Rajendra Jadhav

unread,
Apr 27, 2017, 2:00:14 AM4/27/17
to material...@googlegroups.com
Dear ,

Pls. refer your client approved NDT plan for this joint. Or it may mentioned in drawing also.

regards,
rajendra 

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/384223384.11990334.1493197073009%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

Mac Palola

unread,
Apr 29, 2017, 1:23:06 AM4/29/17
to Materials & Welding, raouf...@yahoo.fr


Sir,

ASME B31.3 - 345.2.3(C) 

Regards