Need guidance for PWHT -
Code of Construction - ASME SEC VIII DIV 1
Job - Heat exchanger
Material - Tube -SA 213 T11 - 19.05 OD X 2.11 THK
Tube sheet - SA 336 F11 CL2 , Cladded with Alloy 600
Tube -Tube sheet joint configuration - Groove and Fillet - 2mm -45Deg Vee with 2 mm fillet
Welding Process proposed - GTAW
Welding filler metal proposed- ERNiC3
Query -
We reviewed the PWHT exemption in Table UCS-56-3 for P-No. 4 materials and UW-40 (f)(g) for Nominal thickness consideration and PWHT requirement
Here nominal thickness is Tube thickness (2.11mm ) as per UW-40 (f)(g)
Pl advice for PWHT exemption for above configuration of Tube to tube sheet PWHT wrt Table UCS-56-3 or any other ref in ASME SEC VIII DIV 1
Thanks
Vishwas - IWE