Dear expert. Please I need your help about the requirements of charpy vee notch toughness for piping and pipeline I mean when the test will be required. I appreciate your help
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4adaf67b-388d-430d-bd1b-95ec89b8dc8f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Dear ,
Its madatory to prepare if service temp is subzero, you may proceed with impact temp below by 5 c as per MDMT.
Regards
Dinesh
Dear expert. Please I need your help about the requirements of charpy vee notch toughness for piping and pipeline I mean when the test will be required. I appreciate your help