STAINLESS STEEL CNTAMINATION

53 views
Skip to first unread message

Ankit Gandhi

unread,
Aug 1, 2016, 10:29:18 PM8/1/16
to Materials & Welding, raghura...@gmail.com, "pgo...@quickclic.net
Dear sir,

Can you suggest any material or coating[in INDIA] on Stainless steel for avoiding contamination during fabrication.

Regards,
Ankit Gandhi

manjunath madiwalar

unread,
Aug 2, 2016, 2:11:33 AM8/2/16
to material...@googlegroups.com
Dear Ankit,
You can wrap gum pu sheet during fabrication to avoid contamination once fully fabricated take out sheet and passivate the whole equipment. Which is cost effective also most of industry follow the same. Gum PU rolls are available in market.
Regards.
Manjunath. T Madiwalar
> --
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
> To post to this group, send email to material...@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ab8289e0-5322-44ff-abbc-eac839165863%40googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
>

Ankit Gandhi

unread,
Sep 25, 2016, 11:58:31 AM9/25/16
to Materials & Welding
Dear sir,

Do you have any brand name or any specification sheet for this product then please inform me on asgan...@gmail.com

Regards,
Ankit