Recommended Paint Specification

34 views
Skip to first unread message

finitei...@gmail.com

unread,
Aug 18, 2022, 3:32:47 AM8/18/22
to Materials & Welding
I need a recommendation for suitable paint specification of internal painting (bottom plate & shell course) of petroleum refinery intermediate product tank with steam coil.

Due to temperature epoxy or polyurethane paint spec may not last.

Rupam Manna

unread,
Aug 18, 2022, 4:46:52 AM8/18/22
to material...@googlegroups.com
Dear Team 
Which electrode I have to use for disimiler E355 & 316 material
Pl suggest 309 or 309L

Thanks & Regards,

Rupam Manna
Mobile:07894459583

Sent from RediffmailNG on Android
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https:roups.google.com/d/msgid/materials-welding/b1c42aaa-3826-47ec...@googlegroups.com.

Reply all
Reply to author
Forward
0 new messages