Groups
Groups
Sign in
Groups
Groups
Materials & Welding
Conversations
Labels
About
Send feedback
Help
Welding AISI 1078
50 views
Skip to first unread message
chris
unread,
Apr 14, 2021, 11:41:59 PM
4/14/21
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
Hello everyone;
Any suggestion for the right filler metal rod for AISI 1078 repair.
Regards
Chris
Vishwas Keskar Welding Manager WELDING
unread,
Apr 15, 2021, 12:08:27 AM
4/15/21
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
What repair actually you intend to do it on AISI 1078
Pl. share MTC, AISI 1078 SPECIFICATION.