Dear experts,
Can we do root by GTAW process, fillup by SMAW process and capping/final by GTAW process?
Any precaution?
If no, why?
steel_microbe
unread,
Jun 13, 2019, 3:58:49 PM6/13/19
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
Yes you can. You can also make weld repairs with your GTAW as long as you do not exceed the 2t qualified for your GTAW process which should be shown on your WPS.