IBR Welding Requirements

160 views
Skip to first unread message

Anand Elankumaran

unread,
Jan 26, 2023, 4:12:13 AM1/26/23
to Materials & Welding
Dear Experts,

Could you please provide the details about the IBR Welding requirements in terms of WPS & PQR, WQT.

--
Thanks and Regards,
E. Anand,
Lead QA-QC,
Sohar,
Oman.

Vishwas Keskar Welding Manager WELDING

unread,
Jan 27, 2023, 12:19:37 AM1/27/23
to Materials & Welding
IBR Regulation 608 onwards specifies  about Welder Qualification certificate.
There is chapter related to  :
QUALIFICATION TESTS FOR WELDERS ENGAGED IN WELDING OF BOILERS AND STEAM-PIPES UNDER CONSTRUCTION, ERECTION AND FABRICATION AT SITE IN INDIA AND IN REPAIRING BOILERS AND STEAM-PIPES BY WELDING

WPS PQR are not required.
Thanks and regards

Vishwas 
IWE 