Cracks on dished end kunkle portion

89 views
Skip to first unread message

Shankar S

unread,
Jan 8, 2016, 12:44:02 AM1/8/16
to Materials & Welding
Dear Experts,

During construction of new refrigeration plant we found LP Receiver on receipt inspection multiple Cracks(6Nos) at knuckle portion of ellipsoidal dished end  with surface depth of crack is ranging from 2mm to 5mm. Thickness of dished end 19mm. measured thickness at the knuckle portion 16.7mm. LP receiver stored for Ammonia. Hydro tested at 24 kg/cm2 as per name plate. Plz through some light to accept/reject/Repaired procedures if any. Code of vessel is ASME Sec VIII, Mtl IS2002/SA516.  

Thanks in advance,
Thanks & Regards,
Shankar Shivaratri,
Hyderabad, India.

Gopalakrishnan G

unread,
Feb 2, 2016, 8:25:25 AM2/2/16
to material...@googlegroups.com

do repair the cracked surface .LPT before and after repair.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a631da90-2732-40b0-b796-687bef80d72d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
G.Gopalakrishnan
Welding Engineer
Mukand Ltd
Mumbai
Moble :+91-9833397917


Reply all
Reply to author
Forward
0 new messages