BUS beam

38 views
Skip to first unread message

basem elabd

unread,
Nov 4, 2020, 9:28:20 PM11/4/20
to material...@googlegroups.com
Dear all

@ built-up section beam in welding SAW progress if the web Thk. equal or less than 8mm.
Can welding from one side only or I can't 

Thanx

Zacharias Rohith Joseph

unread,
Jan 14, 2021, 5:11:44 AM1/14/21
to Materials & Welding
Fillet weld has to be done from both sides.