Tube to tubesheet welding

283 views
Skip to first unread message

venkkatesh krishnan

unread,
May 14, 2015, 4:51:59 AM5/14/15
to material...@googlegroups.com
Dear Experts,

I need to do tube to tubesheet mock up test, as per qw-193 the
thickness of the tubesheet in the mockup test assembly shall be at least as
thick as the production tubesheet, except it is not required to be thicker
than 2 in. (50 mm),


*Existing Design:*Tubesheet thickness is 85mm
Joint Detail: Double groove + expansion and groove with seal welding
Expansion area: full length leaving 3.2mm from back side.

Based on above said point tubesheet exceed 50mm thk there is no need to
same as production coupon, so if i am taking 50mm thickness leaving 3.2mm
from backside and remaining area expansion + welding it's correct
way(expansion area is 47mm),but actual existing expansion area is 82mm, so
I have to take 85mm to mock up test instead of 50mm or go with 50mm
thickness with 47mm only expansion area which one is correct?
I attached 2d drawing of tube to tubesheet joint detail, Kindly clarify my
doubt.


george....@gr.bureauveritas.com

unread,
May 14, 2015, 5:30:58 AM5/14/15
to material...@googlegroups.com

As per QW-193.1, you have to duplicate the tube hole configuration and the tube-to-tubesheet joint design within the limits of the essential variables
 
best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for venkkatesh krishnan ---14/05/2015 11:52:03---Dear Experts,           I need to do tube to tubesheet mvenkkatesh krishnan ---14/05/2015 11:52:03---Dear Experts,           I need to do tube to tubesheet mock up test, as per qw-193 the



From: venkkatesh krishnan <venkkates...@gmail.com>
To: material...@googlegroups.com
Date: 14/05/2015 11:52
Subject: [MW:23281] Tube to tubesheet welding
Sent by: material...@googlegroups.com





Dear Experts,

         I need to do tube to tubesheet mock up test, as per qw-193 the thickness of the tubesheet in the mockup test assembly shall be at least as thick as the production tubesheet, except it is not required to be thicker than 2 in. (50 mm),


Existing Design:


Tubesheet thickness is 85mm
Joint Detail: Double groove + expansion and groove with seal welding
Expansion area: full length leaving 3.2mm from back side.

Based on above said point tubesheet exceed 50mm thk there is no need to same as production coupon, so if i am taking 50mm thickness leaving 3.2mm from backside and remaining area expansion + welding it's correct way(expansion area is 47mm),but actual existing expansion area is 82mm, so I have to take 85mm to mock up test instead of 50mm or go with 50mm thickness with 47mm only expansion area which one is correct?

I attached 2d drawing of tube to tubesheet joint detail, Kindly clarify my doubt.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/ed0751db-4928-4db0-8431-20b4238e30ca%40googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Mohd Azam

unread,
May 14, 2015, 7:40:57 AM5/14/15
to material...@googlegroups.com

If its seal weld then Normal GTAW process WPS as per ASME SEC IX can be used for welding. No need to go for Tube to tube sheet Mock-up.