spherical tank requirements for inspection.

138 views
Skip to first unread message

mervin dio

unread,
Jun 22, 2015, 10:34:31 PM6/22/15
to material...@googlegroups.com
Dear members,

I woluld like to ask a favor from you about the inspection requiremnts for spherical tank iam new for this job i dont have an idea what is the requiremnts Prior to accept the fit up ang after welding.

Regards 

Vin

george....@gr.bureauveritas.com

unread,
Jun 23, 2015, 5:40:56 AM6/23/15
to material...@googlegroups.com

since you are new you have to start studding the applicable construction Code or standard.
If you have any questions on the Code or standard, then you may address the forum.
The forum can not replace Codes and Standards

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Tadic, Miroslav

unread,
Jun 23, 2015, 1:34:48 PM6/23/15
to material...@googlegroups.com

At first, You must identify the construction code of the equipment and then review it.

 

There you´ll have all inspection, examination and testing requirements for the tank  

 

regards

 

Miroslav Tadic

Integrity Enginner
CEE
Gerencia de Producción - Mantenimiento
YPFB Chaco S.A.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1434997585.79550.YahooMailAndroidMobile%40web181503.mail.ne1.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

Prakash Gotimukul

unread,
Jun 23, 2015, 1:35:01 PM6/23/15
to materials-welding
Absolutely correct. This forum will help clarify or have a discussion on interpretation of codes/standards. Members must go thro the codes and raise points for discussion, or a practical problem and possible solutions etc

Rgds
G.Prakash
AIS, AIA LLC TX, USA

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.

agumarca

unread,
Jun 28, 2015, 11:02:17 AM6/28/15
to 'mervin dio' via Materials & Welding

Hi .
If is atmosféric tank is api 650 or 620 for fabrication for inspection is api 653 if is pressure tank is asme section 8 división 1 inspection is NB 23 or api 510 .

Best regars
Agustín Jimenez

El jun 22, 2015 1:26 PM, 'mervin dio' via Materials & Welding <material...@googlegroups.com> escribió:
Dear members,

I woluld like to ask a favor from you about the inspection requiremnts for spherical tank iam new for this job i dont have an idea what is the requiremnts Prior to accept the fit up ang after welding.

Regards 

Vin

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
Reply all
Reply to author
Forward
0 new messages