Dear Experts ,

When i review the ISO 15609 Part-1 for WPS preparation , it does not mention about Procedure Qualification method and testing.
It says only the format to be used for WPS and the necessary datas to be filled in.
So, my query is whether we need to fill the format and send to client for approval, before we start welding.
Is there any other part in ISO 15609 mention about Procedure Qualification and mechanical testing.
The material for the project is JIS SS 304L and the product is venturi tube, only GTAW process we plan to use.
Await for your reply.
Regards
Saravanan
Korea

george....@gr.bureauveritas.com

unread,
Feb 4, 2015, 7:55:12 AM2/4/15
to material...@googlegroups.com

You will find your answers in EN ISO 15614-1
best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for Saravanan Sornam ---04/02/2015 14:25:06---Dear Experts , When i review the ISO 15609 Part-1 for WPS pSaravanan Sornam ---04/02/2015 14:25:06---Dear Experts , When i review the ISO 15609 Part-1 for WPS preparation , it does not

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CALV1rkLv56dqQcvvz3ydgxNfeo9Hc%2B%3DRYx%3D1CmtuBfR7PvcQkQ%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Lab

unread,
Feb 4, 2015, 10:09:37 AM2/4/15
to material...@googlegroups.com

Dear Saravanan,

 

ISO 15614 (it has various parts for different welding) will give you a complete idea about various tests required for qualification of a WPS.

 

Ex. Part 1: Arc and gas welding of steels and arc welding of nickel and nickel alloys

 

PLEASE REFER AND REVRT.

 

Regards,

A Meganathan

Kochi

 

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Saravanan Sornam
Sent: Wednesday, February 4, 2015 4:56 PM
To: material...@googlegroups.com
Subject: [MW:22802] ISO 15609 Part 1- WPS

 

Dear Experts ,

--

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rkLv56dqQcvvz3ydgxNfeo9Hc%2B%3DRYx%3D1CmtuBfR7PvcQkQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


The information contained in this message are Cochin Shipyard Limited confidential and proprietary information and is intended only for the use of the recipient(s) named above. If the reader of this message is not the intended recipient, he/she is hereby notified that any use, dissemination, distribution, or copying of this communication or any of the content is strictly prohibited. In such case, please advise the sender immediately and delete it from your system. Further acknowledges that any views expressed in the message are those of the individual sender and no binding nature of the message shall be implied or assumed unless the sender does so expressly with due authority of Cochin Shipyard Limited.


----------------------------------
Cochin Shipyard Ltd, Cochin, India

Prakash Gotimukul

unread,
Feb 4, 2015, 10:10:01 AM2/4/15
to material...@googlegroups.com
Also see the reference stds given in those EN stds.....

Rgds
G.Prakash
Independent Consultant, ASME AIS/ISO
Technical Director, Hitek Engg Services, Dubai
 gpraka...@gmail.com.

meisam shokri arfaei

unread,
Feb 4, 2015, 10:10:12 AM2/4/15
to material...@googlegroups.com
Dear Saravanan

Please have a look on the scope of the standard. This is mentioned there that, "This standard is part of series of standards....for more information see annex A of ISO 15607-2003.

Annex A of ISO 15607 has a table which define the relationship between all part of those standards.
Also Annexes B & C will be helpful. 

Regards

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rkLv56dqQcvvz3ydgxNfeo9Hc%2B%3DRYx%3D1CmtuBfR7PvcQkQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer





Prakash Gotimukul

unread,
Feb 4, 2015, 11:54:28 AM2/4/15
to material...@googlegroups.com
To the coordinator of MW,
Of late I find that when a question is asked for expert opinion, some individuals are writing with names addressed to the individual who made the question. This is improper. This is a group forum and whatever is written is for all those who contribute and for benefit of all. Some are even asking for a reply etc etc...............
All questions must be generally worded so that any one in the group who wish to answer can do. All answers shd preferably be backed by std references appropriately or by personal experience.
Questions shd not be to resolve personal problems but to enhance and share knowledge. 

Some of my thoughts to improve the groups contribution. I know some of my friends have talked to me and even stopped contributing bcs some where we are not keeping self discipline among ourselves.

Rgds
G.Prakash
Independent Consultant, ASME AIS/ISO
Technical Director, Hitek Engg Services, Dubai
 gpraka...@gmail.com.

MW

unread,
Feb 4, 2015, 12:19:41 PM2/4/15
to material...@googlegroups.com
We fully agree with the concerns raised here, thank you very much for your feedback sir!
in fact there are numerous posts in the forum to request members how to ask and answer a question, but we never tried to stress this issue, how to answer a question.

use meaningful headers/subject line
be precise and informative
If you don't know for sure, say so! A wrong but authoritative-sounding answer is worse than none at all
If you did research to answer the question, demonstrate your skills rather than writing as though you pulled the answer out of your pocket. Answering one good question is like feeding a hungry person one meal, but teaching them research skills by example is teaching them to grow food for a lifetime.

More suggestions are welcome.
Reply all
Reply to author
Forward
0 new messages