Dear All,
According to ASME B31.3, Section 332.2 Bending, flattering or ovality of a bend , the difference between maximum and minimum diameters at any cross section, should not exceed 8% of nominal outside diameter.
Thanks & Regards,
________________________
Faizal R Majeed
QC Piping/Mechanical
Saudi Chevron Phillips Chemical
Office (+966) 13 3568100 Ext.1466
E-mail : fai...@saudichevron.com
P Think Green!!! Please consider your environmental responsibility before printing this e-mail.
From: material...@googlegroups.com [mailto:material...@googlegroups.com]
On Behalf Of M S R K S Prasad
Sent: Thursday, September 01, 2016 9:11 AM
To: material...@googlegroups.com
Subject: [MW:25335] Acceptance for Ovality in mid section of 90 deg Elbow [**EXTERNAL**]
*** WARNING: This email originated outside of the CPChem network. Use caution opening attachments, clicking web links, or replying. ***
-
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/OF37D2BCE3.F801C00A-ON65258021.0021A3C5-65258021.00227D7D%40nagarjunagroup.com.
For more options, visit
https://groups.google.com/d/optout.
From: M S R K S Prasad Sent: Πέμπτη, 1 Σεπτεμβρίου 2016 - 09:33 Reply To: material...@googlegroups.com |
Subject: [MW:25335] Acceptance for Ovality in mid section of 90 deg Elbow |