Dear expert,

I'm having to weld normal duplex plate for vessel, SMAW process with following requirements:

I.v -40degC
FN: 35-65
CPT 22deg C @24 hrs
Corrosion 4g/mm

I'm unable to achieve FN even after several test.

Can anyone guide me how to achieve FN ?

Pravin
Singapore

Sent from my iPhone

meisam shokri arfaei

unread,
Apr 15, 2015, 3:19:09 AM4/15/15
to material...@googlegroups.com
Which test did you implement for measuring the ferrite content?
Ferrite meter equipment or metallography?


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/C06614E3-D0AA-42F0-9BA6-9A63A4690B7C%40gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer





george....@gr.bureauveritas.com

unread,
Apr 15, 2015, 3:22:28 AM4/15/15
to material...@googlegroups.com

You are getting low or high ferrite?

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for Pravin G ---15/04/2015 06:29:23---Dear expert, I'm having to weld normal duplex plate for vessel, SMAPravin G ---15/04/2015 06:29:23---Dear expert, I'm having to weld normal duplex plate for vessel, SMAW process with following requirem

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at


To view this discussion on the web visit

https://groups.google.com/d/msgid/materials-welding/C06614E3-D0AA-42F0-9BA6-9A63A4690B7C%40gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Pravin G

unread,
Apr 15, 2015, 10:18:07 AM4/15/15
to material...@googlegroups.com
Dear Sir,

Our requirement for FN is 35-65, however we are getting exactly 35 which is border line for several test which is unacceptable by the client.

Kindly advice with your expertise.
Pravin Poornachandran


Sent from my iPhone

On 15 Apr 2015, at 15:22, george....@gr.bureauveritas.com wrote:

You are getting low or high ferrite?

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


<graycol.gif>Pravin G ---15/04/2015 06:29:23---Dear expert, I'm having to weld normal duplex plate for vessel, SMAW process with following requirem

Pravin G

unread,
Apr 15, 2015, 10:18:26 AM4/15/15
to material...@googlegroups.com
Dear Sir,

We used ferrite meter equipment.

Pravin Poornachandran


Sent from my iPhone

george....@gr.bureauveritas.com

unread,
Apr 15, 2015, 4:40:05 PM4/15/15
to Pravin G
You weld needs to cool slower to give time for ferrite to develop. Could you send me the process parameters?

Sent from my BlackBerry 10 smartphone.
From: Pravin G
Sent: Τετάρτη, 15 Απριλίου 2015 - 17:18
Subject: Re: [MW:23104] Normal duplex and super duplex


For more options, visit https://groups.google.com/d/optout.

pgoswami

unread,
Apr 16, 2015, 8:22:51 AM4/16/15
to material...@googlegroups.com, htcis...@gmail.com
Hello Pravin,
 
What's the  grade of DSS involved.What's the consumable used and what's the ferrite readings in consumable MTR? What's the thickness involved?
 
Meeting ferrite is only one part of DSS procedure qualification.
 
All those information would be worth looking at.
 
Thanks.
 
 
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineer/Specialist
Ontario, Canada
 


From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Pravin G