Gents
There is a PMI test result which is as follows:
Ni-0.18%, Cr-1.37%, Fe-96.50%, Mn-0.84%, Mo-0.22%. This is a piece of steel pin. Can anyone suggest the rough material grade that this pin has been made off?
Your thoughts will be highly appreciated.
Many thanks
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/HE1PR05MB14334D0F0276A78D94D9CF87EBC40%40HE1PR05MB1433.eurprd05.prod.outlook.com.
For more options, visit https://groups.google.com/d/optout.
It seems to be 4130 but you may further check carbon content to see if it is close to 0.3%.
--