Dear expert,

Anyone can guide me or input regarding new AWS classification of A5.36, I read some welding forum stating from Jan 1st, 2016, A5.20 & A5.29 will be merged and revise to A5.36.

Is this true? If yes, which means all PQR should be revised? Kindly advice and appreciate your help.

Pravin Poornachandran
Singapore