QW-217 (b)

142 views
Skip to first unread message

Emil Tahirzade

unread,
Nov 24, 2023, 6:58:55 AM11/24/23
to Materials & Welding
Dear All,

I want to clarify below mentioned case for which I would like to have your valuable comments:

Case: clad equipment - Base material- CS (P1) 25mm thck,
clad material -- SS 316L , 3 mm thck,
clad provided for corrosion, not included in the design calculation

Welding qualification carried out separately: 1) for base material CS (P1)  2) for restoration of cladding overlay procedure done on CS(P1) for 316L weld. 

 Are these WPSs okay as per QW-217 (b) requirements?

Unfortunately, our ASME AI doesn't agree with me about the second one WPS which cladding overlay with 316L filler material on CS(P1). He says we should prepare WPS for cladding 316L filler material on SS(P8) instead of CS(P1). 

What do you think about it?

Vishwas Keskar

unread,
Nov 24, 2023, 10:34:22 AM11/24/23
to material...@googlegroups.com
In your case Method B is acceptable in line with QW217 .
Pl speak to AI and show the clause with Code
Sent from my iPhone

> On 24-Nov-2023, at 5:28 PM, Emil Tahirzade <emilta...@gmail.com> wrote:
>
> it?

Kannayeram Gnanapandithan

unread,
Nov 24, 2023, 11:51:31 AM11/24/23
to materials-welding
orginal cladding done by weld overly or anyother methods 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/72c02fb9-254b-449e-a2f5-f824ffe4f34fn%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages