Manikandan J

未讀,
2022年2月22日 晚上10:59:212022/2/22
收件者:material...@googlegroups.com
Dear All,

What is the Suitable Consumable for CS to Inconel 625 Material for GTAW & SMAW Material.

Process : GTAW & SMAW

Regards,
Manikandan



james gerald

未讀,
2022年2月23日 凌晨12:16:082022/2/23
收件者:material...@googlegroups.com
ERNiCrMo-3 or ERNiCrMo-10



Inline image
Inline image


Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmNk3ySUGffFw_3pVtosNQj_4AS3S-w9HKS4Bud54qEbDQ%40mail.gmail.com.

George Dilintas

未讀,
2022年2月23日 晚上11:06:482022/2/23
收件者:material...@googlegroups.com
What is matching inconel

Manikandan J

未讀,
2022年2月23日 晚上11:07:122022/2/23
收件者:material...@googlegroups.com
Dear Sir,

Thanks.Can I use ERNiCRFe-2 as per API RP582?


Reagards,
Manikandan.


james gerald

未讀,
2022年2月23日 晚上11:47:152022/2/23
收件者:material...@googlegroups.com
Yes you can. Normally for a higher temperature range and the associated cost.

Inline image

Inline image


Thanks & Regards

J.Gerald Jayakumar


Kannayeram Gnanapandithan

未讀,
2022年2月28日 凌晨3:33:362022/2/28
收件者:materials-welding
NiCrFe2 for high temp & Creep service.  For ur combination ,it is better to use NiCrMo3
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


回覆所有人
回覆作者
轉寄
0 則新訊息