Can a welder use SS electrode on CS material ? for qualification and what is the range?thanks
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/96f58af9-2886-4359-99c7-b6ff1faddbc6n%40googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-jafAFXzgpmm6WtcNSiHTGyv5MspsXxJDPJcJDn8C3hKg%40mail.gmail.com.
On 24-Oct-2023, at 6:42 PM, 'Suraj Naik (KPCL)' via Materials & Welding <material...@googlegroups.com> wrote:
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPTzvScZdDrBtUXGOSMS3b6kA9-cRAstN1n3XA9d7-dbku-aJg%40mail.gmail.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPTzvScZdDrBtUXGOSMS3b6kA9-cRAstN1n3XA9d7-dbku-aJg%40mail.gmail.com.