CLARIFICATION ON PQR DATE

130 views
Skip to first unread message

sathis...@gmail.com

unread,
May 15, 2020, 11:04:55 AM5/15/20
to Materials & Welding
Dear Experts
Kindly clarify below doubt's
Standard: ASME Sec IX

I have conducted procedure qualifications(welding done with recording all parameters) on 10/10/2019 and mechanical testing where conducted on 24/11/2019 in that all the testing were cleared. So my doubt is what date need to be endorsed that is during PQR generated test date or after mechanical test conducted date.

Kindly confirm


Regards.satti

SENTHILKUMAR SWAMINATHAN

unread,
May 16, 2020, 6:23:43 AM5/16/20
to material...@googlegroups.com
Satti, 
Hopefully you have done PQR using proposed WPS. Now you will compile all in one package  (PWPS, Parameters record, NDT, DT, Micro Macro etc..) Final compilation date is well acceptable. 
Regards, 
--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.

Kannayeram Gnanapandithan

unread,
May 16, 2020, 6:23:48 AM5/16/20
to materials-welding
Testing date

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Karthik

unread,
May 16, 2020, 6:24:22 AM5/16/20
to material...@googlegroups.com
--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.

harenath jha

unread,
May 16, 2020, 6:24:27 AM5/16/20
to material...@googlegroups.com
Mechanical test completion date

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Charles Jacob

unread,
May 16, 2020, 6:25:00 AM5/16/20
to material...@googlegroups.com
Dear,
Pqr is valid from the date of welding was performed on the pqr. Date of testing can be on a later date after welding date.

Hope this clarifies.

Regards,

Charles V Jacob

Chandan Singh

unread,
May 16, 2020, 6:25:15 AM5/16/20
to material...@googlegroups.com
Dear,
WQT date is 10/10/2019 and PQR date is 24/11/2019 is correct.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0ae78523-7f75-457f-8941-d8289a5e4d84%40googlegroups.com.
--
Regards
CHANDAN SINGH
Sterling & Wilson 
+919981575817
+917379619175


Reply all
Reply to author
Forward
0 new messages