ASME sect I, Boiler Hydrotest

55 views
Skip to first unread message

Zakaria ghrab

unread,
Jan 19, 2017, 5:43:59 AM1/19/17
to material...@googlegroups.com

Dear all,

  Need your expertise :

Construction code : ASME sect I & ASME B31.1 (Boiler construction project)
Subject : Pressure test on boiler

For boiler hydrotest our contrcator report that for superheater part, pressure etst will be performed at 1.25 MAWP  and not 1.5 MAWP.

ASME sect I, mention about in PG-99.3.1 but is not very clear for me.

Any one can give us interpretation for it please.

Thank you 
--

-----
زكرياء غراب
GHRAB Zakaria 


Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

George Dilintas

unread,
Jan 24, 2017, 9:56:50 PM1/24/17
to Meghanadh K
PT = 1,5XMAWP

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD8EeB2frNCx4iLiPgPMOur%2BryWV6%3DG8pAy-FJCn00U9kzNgMQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

George Dilintas

unread,
Jan 24, 2017, 9:57:00 PM1/24/17
to Meghanadh K
PG-99.3.1 is applicable for a specific type of boilers (forced flow generators with no fixed water lines).

2017-01-19 12:27 GMT+02:00 Zakaria ghrab <zakari...@gmail.com>:

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD8EeB2frNCx4iLiPgPMOur%2BryWV6%3DG8pAy-FJCn00U9kzNgMQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages