Dear Sirs,
Good Day!!!

  My question is Our Company Repairing Marine Boilers So which ASME Codes i can refer for the PWHT&NDT Requirements? I hope anybody guide me on correct way !



Thanks!



George Dilintas

unread,
Dec 12, 2020, 10:07:17 AM12/12/20
to material...@googlegroups.com
Section I

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/95b8c288-ab5e-4f44-af7d-201fa305fe0en%40googlegroups.com.

George Dilintas

unread,
Dec 12, 2020, 10:07:18 AM12/12/20
to material...@googlegroups.com
And NBIC Part 3

Στις Σάβ, 12 Δεκ 2020, 12:30 ο χρήστης Sujith Murali Issac <sujit...@gmail.com> έγραψε:

José Juan Jiménez Alejandro

unread,
Dec 13, 2020, 11:02:19 PM12/13/20
to material...@googlegroups.com
The ASME Code is for new equipment manufactured in a plant that must have ASME Stamp, but repairs (generally in equipment in use) must be done with the NB-23 of the NBIC (Stamp R), you must rely on Code Y Edition with which the boiler you are repairing was manufactured (ASME Section I in this case), in the NB-23 you will find a series of step-by-step recommendations so that you can repair the boiler without major problems, it is a Code very good and little known, Dr. George Dilintas is absolutely right.
Cheers!.



--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SUMMIT MÉXICO - TPI

https://www.linkedin.com/in/summit-m%C3%A9xico-tpi-760047137/

Móvil +52 1 812 352 4606

Skype: jjjimeneza





Reply all
Reply to author
Forward
0 new messages