API steels may be welded to DSS as support , under proper cathodic protection environments, not as direct Butt-Joints with the same process parameter envelopes.
Thanks.
P.Goswami.P.Eng, IWE.
Independent Welding & Metallurgical Specialist
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
Email:pgos...@quickclic.net,pradip....@gmail.com
Cell/Whasapp:1-905-9793232
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/70916cb3-d5d3-4952-8d0c-aebe10c76f40%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
ASME SFA 5.4, Classification E2209—duplex filler material. |
ASME SFA 5.4, Classification E309L—high-alloy austenitic filler material |
ASME SFA 5.4, Classification E309LMo—high-alloy austenitic filler material |
--
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUjWDn5WS%3D0f2fVjyHpohAiEKknEDELqpxaHKukqJxhAXg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40DK2HsKHtPeHKHUcvtfL%2BsfHEFEh3NB3dnZU-jJoXTcSg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.