Machining allowed in Butt weld pressure joint?

41 views
Skip to first unread message

Vadivel Mahadevan

unread,
Sep 7, 2016, 6:12:06 AM9/7/16
to Materials & Welding, VADIVEL MAHADEVAN
Dear Experts!!

I am from a Valve industry. I am doing fabrication of a valve. After butt welding of two plates, can I carry out skin machining till the plate surface, so that welding is not seen..

I follow ASME Sec.IX for welding qualification.
What are the factors i am supposed to consider.

Thanks and regards
Vadivel. M

Ankit Gandhi

unread,
Sep 13, 2016, 7:29:21 AM9/13/16
to Materials & Welding, vadivel...@gmail.com
Dear
You can do machining on seam bbut after machining you have to follow ndt requirement.
For your satisfaction and reduce rework you can carried out ndt before machining but after machining NDT is required.
ASME SEC. IX not restrict m/c.

Regards,
Ankit Gandhi

George Dilintas

unread,
Sep 13, 2016, 10:48:48 PM9/13/16
to Meghanadh K
Yes, you do


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/536f54af-8077-458c-b4d0-b6325c1b0da1%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

c sridhar

unread,
Sep 17, 2016, 8:09:36 AM9/17/16
to material...@googlegroups.com
U have not mentioned the thickness of the plate.

Is it single 'V' weld a seal pass after groove grinding and dp check.to avoid
ucs, slag or pores. If it is a double'V' no problem. U can go ahead.

Sridhar, .


From: George Dilintas <dili...@gmail.com>
To: Meghanadh K <material...@googlegroups.com>
Sent: Tuesday, 13 September 2016 5:49 PM
Subject: Re: [MW:25387] Re: Machining allowed in Butt weld pressure joint?

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40D%3D9WRUQXxwzgqh5SP%2BGYT0bVOw0BkoA_%2ByK%2BrSepZy-A%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages