Kindly suggest suitable filler wire for following base metal combination.

 

 

      Parent Metal 1                                  Parent metal 2

 

1)   ASTM A 217 GR C 5         ASTM A 217 GR CA15

2)   ASTM A 217 GR C 12       ASTM A 217 GR CA15

3)   ASTM A 217 GR WC 6      ASTM A 217 GR CA15

4)   ASTM A 217 GR WC 9      ASTM A 217 GR CA15

 

Thanks &  Regards,

Brajendra  S Patel  | Engineer -Welding

 

Mob:+917057406907

 

 

 

 

 

 

 

 

 

 

 

 

 

 

Help save the environment - do you really need to print this e-mail?

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 


Think before you print. This e-mail may contain confidential and privileged material for the sole use of the intended recipient. Any review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient (or authorized to receive for the recipient), please contact the sender by reply e-mail and delete all copies of this message. Koso India Pvt Ltd. --- H-33 & 34, MIDC, Ambad, Nashik – 422010, Maharashtra, India ,Tel + 91 253 2408811, Fax + 91 253 2384413.

George Dilintas

unread,
Nov 13, 2016, 9:20:36 PM11/13/16
to Meghanadh K
Go to SFA 5.5 and choose among the grades listed their in those which much the properties of the various grades of SA-217

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/D288AF0A8981664D8CC97F6CFF20756B388557C2%40XCELLMBX01.xcellinfra.india.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages