         Can anyone tell us formula for tank shell plate life calculation.
Shell plate thickness initial 20mm
shell plate thickness after 15 years 19mm. Corrosion allowance 1.5 mm.

KVN Rao

chandrakant mohikar

unread,
Mar 1, 2017, 2:26:46 AM3/1/17
to material...@googlegroups.com


Shell has some imp aspects & components like Design considerations & requirements, plate arrangements,  joints, compression at joint at she'll n roof, & at btm,  nozzles,  80+mm nozzles,  wldg of she'll btm, upper n lower she'lls. 

u may elaborate specific requirements

Chandrakant Mohikar (ex. PDO, Area Project QA )

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGJWGdN7P8fw4%2BFyt-uo5G7zsCcV0YNxnav1L5%2BCxphT3xEu-g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Dinesh Somwanshi

unread,
Mar 1, 2017, 2:26:50 AM3/1/17
to materials-welding
Dear pls,

go with API 653


*DINESH VITTHAL SOMWANSHI*

*BACHELOR IN MECHANICAL ENGINEER*

*AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL,*
*API 570 - Piping Inspector,** AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3*
*NDT II -UT , RT , MT , PT, VT*
00919881344135
Skype = dinesh570_1

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*


--

George Dilintas

unread,
Mar 1, 2017, 9:41:48 PM3/1/17
to Meghanadh K
You need to know the corrosion rate of the stored fluid in the tank.
Some times the corrosion is linear in time, some times not.
Considering the corrosion rate observed during the last 15 years, you should monitor the thickness every 3 years

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGJWGdN7P8fw4%2BFyt-uo5G7zsCcV0YNxnav1L5%2BCxphT3xEu-g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages