PWHT of branch connections.

60 views
Skip to first unread message

Hareesh K V

unread,
Mar 17, 2016, 11:28:02 PM3/17/16
to materials-welding
Dear Sir,

As per ASME B31.3, for branch connections, PWHT is to be done for the entire circumference of main pipe. Is there any exceptions/code interpretations for that, in Carbon steel material or Alloy steel material (SA335 Gr P9,95)?

For example: A 3/4" branch is done on the main pipe of 60" dia. As per the code requirement, the entire 60" dia is to be wrapped with coil and PWHT is to be done.

Thanks in advance.

Regards,

Hareesh K V
+91-8547859202

--
----------------------
Hareesh K V
+91-9447625012


afrozsh...@gmail.com

unread,
Mar 18, 2016, 10:21:56 PM3/18/16
to Materials & Welding
Dear Harish,

Please reffer AWS D10.10 FIG 6 (PWHT Pratice for branch connection to Pipe attachment weld )

Regards,

Afroz Shaikh

George Dilintas

unread,
Mar 22, 2016, 11:24:52 AM3/22/16
to Meghanadh K
the code use the term "shall" (in other sections also).
To the best of  my knowledge no execption

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAWX5nLOPkVL5UxS5uRTSO%3DKj%3DuWk6bmYbmkkJO%2BnQMy_A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages